Attribute | Value |
---|---|
Packing | Ply-wooden Case With Iron Frame |
Base Pipe Material | P9, P22 |
Welding Type | HFW, serrated |
Production Process | Cold Drawn |
Operating Temperature | 300℃ |
Fin Thickness | 1.8-3mm |
NDT | ET, HT |
The ASTM A213 T22 Alloy Steel Serrated Fin Tube is designed for high-temperature applications in furnace convection sections and other thermal systems. The base tube is made from T22 alloy steel, and the serrated carbon steel fins are welded onto the tube surface. The serrated fin design increases the surface area, promoting efficient heat transfer and making it suitable for applications where high thermal efficiency and durability are required.
Element | Content (%) |
---|---|
C | 0.08-0.15 |
Mn | 0.30-0.60 |
P | ≤ 0.025 |
S | ≤ 0.025 |
Si | 0.50-0.80 |
Cr | 2.00-2.50 |
Mo | 1.00-1.20 |
Fe | Balance |
Property | Value |
---|---|
Tensile Strength | ≥ 415 MPa |
Yield Strength | ≥ 205 MPa |
Elongation | ≥ 30% |
Hardness | ≤ 192 HB |
Max Operating Temp | ~ 600°C (1112°F) |
Element | Content (%) |
---|---|
C | ≤ 0.22 |
Mn | 0.30-0.70 |
P | ≤ 0.045 |
S | ≤ 0.050 |
Fe | Balance |
ব্র্যান্ড নাম: | Yuhong |
মডেল নম্বর: | ASTM A213 T22 |
MOQ: | 100 কেজি |
দাম: | Negotiate |
প্যাকেজিংয়ের বিবরণ: | লোহার ফ্রেম সহ প্লাই-কাঠের কেস |
অর্থ প্রদানের শর্তাবলী: | এল/সি, টি/টি |
Attribute | Value |
---|---|
Packing | Ply-wooden Case With Iron Frame |
Base Pipe Material | P9, P22 |
Welding Type | HFW, serrated |
Production Process | Cold Drawn |
Operating Temperature | 300℃ |
Fin Thickness | 1.8-3mm |
NDT | ET, HT |
The ASTM A213 T22 Alloy Steel Serrated Fin Tube is designed for high-temperature applications in furnace convection sections and other thermal systems. The base tube is made from T22 alloy steel, and the serrated carbon steel fins are welded onto the tube surface. The serrated fin design increases the surface area, promoting efficient heat transfer and making it suitable for applications where high thermal efficiency and durability are required.
Element | Content (%) |
---|---|
C | 0.08-0.15 |
Mn | 0.30-0.60 |
P | ≤ 0.025 |
S | ≤ 0.025 |
Si | 0.50-0.80 |
Cr | 2.00-2.50 |
Mo | 1.00-1.20 |
Fe | Balance |
Property | Value |
---|---|
Tensile Strength | ≥ 415 MPa |
Yield Strength | ≥ 205 MPa |
Elongation | ≥ 30% |
Hardness | ≤ 192 HB |
Max Operating Temp | ~ 600°C (1112°F) |
Element | Content (%) |
---|---|
C | ≤ 0.22 |
Mn | 0.30-0.70 |
P | ≤ 0.045 |
S | ≤ 0.050 |
Fe | Balance |